内禀矫顽力(Hcj):1592-1990 kA/m |
内禀矫顽力温度系数(β(Hcj)):0.15-0.20 %/°C |
剩磁(Br):0.80-1.14 T |
剩磁温度系数(α(Br)):0.011-0.039 %/°C |
居里温度(Tc):800-840 °C |
工作温度(Tw):300-350 °C |
最大磁能积((BH)max):119-271 kJ/m³ |
磁感应强度矫顽力(Hcb):589-845 kA/m |
制作工艺:Sintered; Bonded; Injection Molding |
材料:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitrogen |
工作温度范围(放大器单元):300 ~ 350 ℃ |
Curie Temperature:800 ~ 840 ℃ |
Intrinsic Coercivity:1200 ~ 1990 kA/m |
Intrinsic Coercivity Temperature Coefficient:0.15 ~ 0.20 -%/℃ |
Maximum Energy Product:119 ~ 271 kJ/m³ |
Residual Magnetism:0.80 ~ 1.52 T |
Residual Magnetism Temperature Coefficient:0.011 ~ 0.039 -%/℃ |
Curie Temperature (Tc):800 ~ 840 °C |
Intrinsic Coercivity (Hcj):1592 ~ 1990 kA/m |
Intrinsic Coercivity Temperature Coefficient (β(Hcj)):0.15 ~ 0.20 -%/°C |
Magnetic Induction Coercivity (Hcb):589 ~ 845 kA/m |
Maximum Energy Product ((BH)max):119 ~ 271 kJ/m³ |
Operating Temperature (Tw):300 ~ 350 °C |
Remanence (Br):0.80 ~ 1.52 T |
Remanence Temperature Coefficient (α(Br)):0.011 ~ 0.039 -%/°C |
材料:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitride |
工作温度范围(放大器单元):300 ~ 350 °C |
Curie Temperature:800 ~ 840 °C |
Intrinsic Coercivity:1592 ~ 1990 kA/m |
Intrinsic Coercivity Temperature Coefficient:0.15 ~ 0.20 /°C |
Max Energy Product:119 ~ 271 kJ/m³ |
Process:Sintered; Bonded; Injection Molding; Injection Molding |
Remanence:0.80 ~ 1.14 T |
Remanence Temperature Coefficient:0.011 ~ 0.039 /°C |
居里温度:800 ~ 840℃ |
内禀矫顽力温度系数(β(Hcj)):0.15 ~ 0.20 /°C |
工艺分类:Sintered; Bonded; Injection Molding |
最大磁能积((BH)max):119 ~ 271 kJ/m³ |
工作温度:300 ~ 350℃ |
剩磁温度系数(α(Br)):0.011 ~ 0.039 /°C |
Intrinsic Coercivity Minimum:1592 ~ 1990 kA/m |
Material Type:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitride |
Remanence Minimum:0.80 ~ 1.14 T |
制作工艺:Sintered; Bonded; Injection Molding |
工作温度范围(放大器单元):300 ~ 350 ℃ |
Curie Temperature:800 ~ 840 ℃ |
Intrinsic Coercivity:1200 ~ 446 kA/m |
Intrinsic Coercivity Temperature Coefficient:0.011 ~ 0.039 %/℃ |
Material Classification:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitride |
Maximum Energy Product:15 ~ 58 kJ/m³ |
Residual Magnetism:0.80 ~ 1.52 T |
Residual Magnetism Temperature Coefficient:0.15 ~ 0.20 %/℃ |