居里温度:800 ~ 840 ℃ |
内禀矫顽力(Hcj):1592 ~ 2130 kA/m |
内禀矫顽力温度系数(β(Hcj)):0.15 ~ 0.20 -%/℃ |
材料:Samarium Cobalt; Neodymium Iron Boron; Ferrite; Samarium Iron Nitride |
最大磁能积((BH)max):119 ~ 446 kJ/m³ |
工作温度:300 ~ 350 ℃ |
剩磁(Br):0.80 ~ 1.52 T |
剩磁温度系数(α(Br)):0.011 ~ 0.039 -%/℃ |
工艺分类:Sintered; Bonded; Injection Molding; Injection Molding |
Curie Temperature Tc:800 ~ 840 ℃ |
Intrinsic Coercivity Hcj:1592 ~ 1990 kA/m |
Intrinsic Coercivity Temperature Coefficient β(Hcj):0.15 ~ 0.20 -%/℃ |
Magnetic Induction Coercivity Hcb:589 ~ 845 kA/m |
Material Classification:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitride |
Maximum Energy Product (BH)max:119 ~ 271 kJ/m3 |
Operating Temperature Tw:300 ~ 350 ℃ |
Remanence Br:0.80 ~ 1.14 T |
Remanence Temperature Coefficient α(Br):0.011 ~ 0.039 -%/℃ |