工艺分类:Sintered; Bonded; Injection Molding; Injection Molding |
材料:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitride |
工作温度:300 ~ 350 ℃ |
形状:Customizable |
Curie Temperature Tc:800 ~ 840 ℃ |
Intrinsic Coercivity Hcj:1200 ~ 446 kA/m |
Intrinsic Coercivity Temperature Coefficient β(Hcj):0.15 ~ 0.20 /°C |
Maximum Energy Product (BH)max:119 ~ 271 kJ/m³ |
Remanence Br:0.80 ~ 1.52 T |
Remanence Temperature Coefficient α(Br):0.011 ~ 0.039 /°C |
材料:Ferrite; Samarium Cobalt; Neodymium Iron Boron; Samarium Iron Nitride |
工作温度范围(放大器单元):300 ~ 350℃ |
形状:Customizable |
Curie Temperature:800 ~ 840℃ |
Intrinsic Coercivity:1200 ~ 446kA/m |
Intrinsic Coercivity Temperature Coefficient:0.15 ~ 0.20/°C |
Maximum Energy Product:119 ~ 271kJ/m³ |
Process:Sintered; Bonded; Injection; Injection Molding |
Residual Magnetic Flux Density:0.80 ~ 1.52T |
Residual Magnetic Flux Density Temperature Coefficient:0.011 ~ 0.039/°C |